Drilling FTO Coated Glass – FTO Coated Glass (CTE substrate dependent, 80 – 82% visible @ 7 ohm/sq); Drilling to +/-0.02 mm hole position. No minimum order; DFM review included with every RFQ.
Ask any process engineer what makes fto coated glass difficult and the answer is specific: the harder FTO film abrades diamond tooling faster and edges need post-cut inspection for film lift. Our drilling line is tooled around exactly that – diamond core drills, ultrasonic assist and laser percussion heads – holding +/-0.02 mm hole position on parts from 0.1 – 30 mm thick.
Specification envelope
| Material | FTO Coated Glass (TEC-7, TEC-15 equivalents) |
|---|---|
| Thermal expansion (CTE) | substrate dependent |
| Service temperature | 600 C (coating stable) |
| Transmission range | 80 – 82% visible @ 7 ohm/sq |
| Density | 2.23 – 2.50 g/cm3 |
| Knoop hardness | harder film than ITO |
| Refractive index | ~2.0 (FTO film) |
| Stock thickness | 1.1 – 3.2 mm substrates |
| Maximum blank size | 360 x 300 mm |
| Process | Drilling |
| Working tolerance | +/-0.02 mm hole position |
| Minimum feature | 0.15 mm laser / 0.5 mm mechanical |
| Surface finish | exit-chip controlled below 0.1 mm |
| Thickness window | 0.1 – 30 mm |
| Edge condition | optional chamfered hole entry |
| RFQ inputs | PDF/DXF/STEP drawing, quantity brackets, surface and edge spec |
Process window
Drilling earns its place through through-holes, blind holes and countersinks at densities beyond 1,000 holes per part. Its boundary condition – hole-to-edge distance should stay above 1.5x thickness to protect strength – is the first thing our DFM review checks.
Beyond this page, FTO Coated Glass routinely runs through dicing, etching, coring, edge grinding in our shop – most real parts combine two or three of these steps.
Specification advice
Before sending the RFQ, check these against your drawing:
- Material note: the harder FTO film abrades diamond tooling faster and edges need post-cut inspection for film lift.
- Process boundary: hole-to-edge distance should stay above 1.5x thickness to protect strength.
- Over-specification is the quiet budget killer: a 20/10 scratch-dig face costs roughly three times an 80/50 face, so grade each surface individually.
For the complete framework, see the tolerance design guide and the holes and edges design guide.
Who orders this
drilling fto coated glass shows up across scientific instruments (reference flats, cells, prism mounts, stage inserts); machine vision (camera windows, ring-light diffusers, calibration plates); laboratory instruments (cuvettes, sight glasses, stir-cell windows). Background reading on the underlying material science: ScienceDirect: FTO glass.
Dimensions still moving? Configure this part live in the 3D + 2D builder below, or open the full custom glass machining 3D + 2D builder to start from a blank canvas.
Useful companion pages: custom FTO glass, FTO conductive glass, machining tolerance guide.
Buyer questions, answered
How fast can prototypes ship?
Machined prototypes ship in 5 – 10 working days. Coated or bonded parts add 1 – 2 weeks depending on queue slots.
What files do you need for a quote?
A dimensioned PDF plus DXF or STEP geometry. If only a sketch exists, our drawing review service formalizes it before quoting.
Do parts ship with inspection data?
Dimensional reports, surface certificates and material certs per melt are available; specify the level on the RFQ.
What tolerances are achievable on FTO Coated Glass parts?
Ground features hold +/-0.01 mm and lapped thickness reaches +/-0.003 mm. The harder FTO film abrades diamond tooling faster and edges need post-cut inspection for film lift.