Edge Grinding FTO Coated Glass – FTO Coated Glass (CTE substrate dependent, 80 – 82% visible @ 7 ohm/sq); Edge Grinding to chamfer +/-0.05 mm. No minimum order; DFM review included with every RFQ.
We edge-grind FTO Coated Glass daily, in thicknesses from 0.1 – 25 mm. The controlling numbers: chamfer +/-0.05 mm working tolerance, 0.1 mm chamfer leg minimum features, and ground C or R profile, polish option off the machine. Where the drawing asks for more, downstream lapping and polishing take over.
Specifications at a glance
| Material | FTO Coated Glass (TEC-7, TEC-15 equivalents) |
|---|---|
| Thermal expansion (CTE) | substrate dependent |
| Service temperature | 600 C (coating stable) |
| Transmission range | 80 – 82% visible @ 7 ohm/sq |
| Density | 2.23 – 2.50 g/cm3 |
| Knoop hardness | harder film than ITO |
| Refractive index | ~2.0 (FTO film) |
| Stock thickness | 1.1 – 3.2 mm substrates |
| Maximum blank size | 360 x 300 mm |
| Process | Edge Grinding |
| Working tolerance | chamfer +/-0.05 mm |
| Minimum feature | 0.1 mm chamfer leg |
| Surface finish | ground C or R profile, polish option |
| Thickness window | 0.1 – 25 mm |
| Edge condition | C-chamfer, R-round, pencil or OG profile |
| RFQ inputs | PDF/DXF/STEP drawing, quantity brackets, surface and edge spec |
Capabilities and limits
The core strength of Edge Grinding is edge strength – a finished chamfer roughly doubles the bend strength of a cut edge. The honest limit: profiles below 0.1 mm leg length are lapped by hand and priced per edge. Both belong on the drawing before quoting, not after.
One material, many routes: on FTO Coated Glass we also quote coring, dicing, drilling, and multi-step drawings are the norm rather than the exception.
Specification advice
Before sending the RFQ, check these against your drawing:
- Material note: the harder FTO film abrades diamond tooling faster and edges need post-cut inspection for film lift.
- Process boundary: profiles below 0.1 mm leg length are lapped by hand and priced per edge.
- Over-specification is the quiet budget killer: a 20/10 scratch-dig face costs roughly three times an 80/50 face, so grade each surface individually.
For the complete framework, see the tolerance design guide and the holes and edges design guide.
Where these parts end up
edge grinding fto coated glass shows up across microfluidic devices (chips, manifolds, via plates, bonded stacks); led packaging (groove covers, phosphor carriers, package windows); semiconductor equipment (view ports, wafer carriers, plasma rings, chamber windows). Background reading on the underlying material science: ScienceDirect: FTO glass.
Dimensions still moving? Configure this part live in the 3D + 2D builder below, or open the full custom glass machining 3D + 2D builder to start from a blank canvas.
For adjacent specifications, see edge grinding overview, holes and edges design guide, ultra-thin glass materials.
Buyer questions, answered
How fast can prototypes ship?
Machined prototypes ship in 5 – 10 working days. Coated or bonded parts add 1 – 2 weeks depending on queue slots.
What files do you need for a quote?
A dimensioned PDF plus DXF or STEP geometry. If only a sketch exists, our drawing review service formalizes it before quoting.
Do parts ship with inspection data?
Dimensional reports, surface certificates and material certs per melt are available; specify the level on the RFQ.
What tolerances are achievable on FTO Coated Glass parts?
Ground features hold +/-0.01 mm and lapped thickness reaches +/-0.003 mm. The harder FTO film abrades diamond tooling faster and edges need post-cut inspection for film lift.
Specifications on this page were last reviewed by our engineering team in September 2026.