Quick answer: Drilling Borofloat 33 covers Borofloat 33 (CTE 3.25 x 10^-6 /K, 350 nm – 2.0 um); Drilling to +/-0.02 mm hole position. Prototypes ship in 5-10 working days.
Ask any process engineer what makes borofloat 33 difficult and the answer is specific: float tin side must be tracked when parts see coating or bonding steps. Our drilling line is tooled around exactly that – diamond core drills, ultrasonic assist and laser percussion heads – holding +/-0.02 mm hole position on parts from 0.1 – 30 mm thick.
Specification envelope
| Material | Borofloat 33 (SCHOTT float production, wafer grade) |
|---|---|
| Thermal expansion (CTE) | 3.25 x 10^-6 /K |
| Service temperature | 450 C continuous |
| Transmission range | 350 nm – 2.0 um |
| Density | 2.23 g/cm3 |
| Knoop hardness | 480 kg/mm2 |
| Refractive index | 1.471 @ 587 nm |
| Stock thickness | 0.70 – 25.4 mm |
| Maximum blank size | 500 x 500 mm |
| Process | Drilling |
| Working tolerance | +/-0.02 mm hole position |
| Minimum feature | 0.15 mm laser / 0.5 mm mechanical |
| Surface finish | exit-chip controlled below 0.1 mm |
| Thickness window | 0.1 – 30 mm |
| Edge condition | optional chamfered hole entry |
| RFQ inputs | PDF/DXF/STEP drawing, quantity brackets, surface and edge spec |
What the process holds
Drilling earns its place through through-holes, blind holes and countersinks at densities beyond 1,000 holes per part. Its boundary condition – hole-to-edge distance should stay above 1.5x thickness to protect strength – is the first thing our DFM review checks.
Beyond this page, Borofloat 33 routinely runs through polishing, grinding, dicing in our shop – most real parts combine two or three of these steps.
Design guidance
The shop-floor rules that matter here:
- Material note: float tin side must be tracked when parts see coating or bonding steps.
- Process boundary: hole-to-edge distance should stay above 1.5x thickness to protect strength.
- Over-specification is the quiet budget killer: a 20/10 scratch-dig face costs roughly three times an 80/50 face, so grade each surface individually.
The full rules live in our tolerance design guide and holes and edges design guide.
Where these parts end up
drilling borofloat 33 shows up across microfluidic devices (chips, manifolds, via plates, bonded stacks); machine vision (camera windows, ring-light diffusers, calibration plates); optical sensors (sensor windows, filter caps, lens covers). Background reading on the underlying material science: SCHOTT BOROFLOAT product page.
Dimensions still moving? Configure this part live in the 3D + 2D builder below, or open the full custom glass machining 3D + 2D builder to start from a blank canvas.
Useful companion pages: 4 inch Borofloat wafers, wafer dicing process, surface quality guide.
Frequently asked questions
How fast can prototypes ship?
Machined prototypes ship in 5 – 10 working days. Coated or bonded parts add 1 – 2 weeks depending on queue slots.
What files do you need for a quote?
A dimensioned PDF plus DXF or STEP geometry. If only a sketch exists, our drawing review service formalizes it before quoting.
Do parts ship with inspection data?
Dimensional reports, surface certificates and material certs per melt are available; specify the level on the RFQ.
What tolerances are achievable on Borofloat 33 parts?
Ground features hold +/-0.01 mm and lapped thickness reaches +/-0.003 mm. Float tin side must be tracked when parts see coating or bonding steps.